Electron diffraction studies indicated that the aging of freshly deposited nickel or activated platinum was at least in part caused by changes in crystal structure. Confirmation was also obtained for the idea that the different forms of hydrogen on platinum are hydrogens adsorbed on different crystal planes. -c partial of hydrogen sulfidation of partial of